摘要本篇论文主要通过本体法,研究制备了发泡均匀的聚甲基丙烯酰亚胺(PMI)泡沫 塑料。首先以甲基丙烯酸(MAA)、丙烯腈(AN)为主要单体,用偶氮二异丁腈(AIBN)作为引发剂,用丙烯酰胺(AM)作为交联剂,用甲酰胺作为发泡剂,用碳 酰胺作为成核剂,通过本体聚合的方法制备出 MAA/AN 共聚物,然后进行发泡制得 PMI 泡沫塑料。然后用光学显微镜和扫描电子显微镜(SEM)观察了泡孔结构,用傅 里叶红外光谱(FTIR)分析了 PMI 共聚发泡过程中的分子结构变化,并用万能拉伸试 验机测试了泡沫的压缩性能,最后分别用动态热机械分析(DMA)、差示扫描量热仪 法(DSC)、热失重分析(TGA)以及热变形温度测试(HDT)研究了 PMI 泡沫塑料 的热性能。83365

研究结果表明:58 份 AN、42 份 MAA、2~3 份丙烯酰胺、0。2~0。3 份 AIBN、5 份甲 酰胺、2 份碳酰胺的配方组成,可以制备出发泡均匀的 PMI 泡沫塑料;泡孔均为闭孔 结构,大小均一。共聚物在发泡过程中生成了酰亚胺环状结构,以及一小部分的酸酐 结构和少部分的梯形结构;PMI 泡沫塑料的压缩屈服应力为 1。319 MPa,压缩强度为 1。591 MPa,压缩时泡孔由外及内逐层破坏;DMA 和 DSC 所测 PMI 泡沫塑料的玻璃化 温度  分别为 178   和 225   。PMI 泡沫塑料的热变形温度(HDI)为 211 。TGA 分析 PMI 泡沫塑料的热分解温度为 315  。

毕业论文关键字:聚甲基丙烯酰亚胺;泡沫塑料;制备;性能

Abstract In this paper, we mainly study the preparation of foam-uniform polymethacrylimide (PMI) foam plastic。 First, using methacrylic acid (MAA) and acrylonitrile (AN) as main monomers, with azobisisobutyronitrile (AIBN) as initiator, acrylamide (AM) as crosslink agent, formamide as foaming agent, carbonamide as nucleating agent, by bulk polymerization prepared MAA/ AN copolymer, then foaming become PMI foam plastic。 Then, the cell structure was observed by optical microscope and a scanning electron microscope (SEM), by Fourier transform infrared spectroscopy (FTIR) analysis the molecular structure changes in the foaming process of PMI copolymerization, and also test the foam compression performance。 Finally, the dynamic mechanical thermal analysis (DMA), differential scanning calorimetry (DSC), thermal gravimetric analysis (TGA) and heat deformation temperature (HDT) test to study the thermal properties of PMI foam on a universal tensile testing machine。

The results of the study show that: the prescription containing 58 phr。AN , 42 phr。MAA , 2~3 phr。AM , 0。2~0。3 phr。AIBN , 5 phr。formamide , 2 phr。carbonamide can be prepared

foam-uniform PMI foam plastics ; The foam cell are closed, uniform size。 In the foaming process of the copolymer generates the cyclic hexahydroxy imide structure, less part of the ladder structure and the acid anhydride structure; The compression yield stress of PMI foam plastic is 1。319MPa, and the compression strength is 1。591MPa, PMI foam plastic is damaged from outside to inside layer by layer; The glass transition temperature  of PMI foam plastic measured by DMA and DSC are 178   and 225    , respectively。 The HDI of PMI foam plastic is 211 。 The thermal decomposition temperature of PMI foam plastic is 315    。

Keywords: Polymethacrylimide;Foamed plastics;Preparation; Performance

第一章 绪论 1

1。1  泡沫塑料 1

1。1。1  泡沫塑料的分类 1

1。1。2  泡沫塑料的成型原理 1

1。1。3  泡沫塑料的制备方法

上一篇:机器人MAG对接仰焊打底焊工艺研究
下一篇:烯丙基聚氧乙烯醚基马来酸酐共聚物超塑化剂的制备

智能自愈合多聚糖水凝胶的性能研究

微发泡注射成型PP/HDPE聚合...

交联凝胶聚合物电解质的制备及性能研究

具有双纳米构造的聚偏氟...

聚多巴胺微胶囊的结构与特性

胶体金免疫层析法检测D-二聚体的研究

聚硼硅氧烷对PC/PBT合金的阻燃作用

大规模MIMO系统的发展研究现状

MNL模型历史城区居民活动...

遥感土地用变化监测国内外研究现状

浅析施工企业保理融资成...

提高小學语文課堂朗读教...

高效课堂教师问卷调查表

从企业eHR建设谈管理信息...

《水浒传》中血腥暴力研...

PCI+PID算法直流力矩电机速...

小型通用机器人控制系统设计任务书